24. Solving a chemistry problem
Sold <10
0 000 X
There are no such quantities in stock
By clicking the button, you agree to
terms for buyers
Secure deal
Instant delivery
Product description
4.12 The electrolytic nickel plating process is carried out at a cathodic current density of 4.0 A/dm2 with a current efficiency of 96%. The layer thickness on the parts is 25 microns. Calculate the duration of the process when nickel plating 1 m2 of parts; power consumption at bath voltage 5.0 and voltage loss 10%; (Ni2+).
Main features
- Content type File
- Content description 17,29 kB
- Updated on the site 16.05.2024
Additional description
If you cannot open the file or have any problems, do not rush to leave a negative review! Contact me and I will quickly help you solve the problem. After purchasing, please leave a positive review of the product :)
Reviews
No reviews yet
0 000 X
There are no such quantities in stock
By clicking the button, you agree to
terms for buyers
Secure deal
Instant delivery
You viewed
All images, logos, and names of games, programs, and other products used are taken from public sources and are for informational purposes only. All trademarks, logos, names, and other intellectual property belong to their respective owners. Use of such images on the website does not imply any affiliation or connection with the copyright holders.